Technique
87 micrographs for technique Scanning electron microscopy (SEM), ordered by micrograph number.
Showing 61 - 70 of 87 micrographs | Page 1 .. 3 4 5 6 7 8 9 | Previous | Next |
Micrograph
626
:
Glass fibre reinforced thermoplastic matrix composite System: Glass fibre composite, Composition: Polypropylene matrix with glass fibre Scanning electron microscopy (SEM) 60 μm |
|
Micrograph
627
:
Glass fibre reinforced thermoplastic matrix composite System: Glass fibre composite, Composition: Polypropylene matrix with glass fibre Scanning electron microscopy (SEM) 200 μm |
|
Micrograph
628
:
Sintered salt (NaCl) System: Na-Cl, Composition: Not specified Scanning electron microscopy (SEM) 140 μm |
|
Micrograph
635
:
Open celled aluminium foam produced by infiltration of sintered salt System: Al, Composition: Not specified Scanning electron microscopy (SEM) 400 μm |
|
Micrograph
640
:
Fracture surface in a liquid crystalline polymer, oriented by a magnetic field System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14401 Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
641
:
Fracture surface in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14401 Scanning electron microscopy (SEM) 12 μm |
|
Micrograph
642
:
Fracture surface in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14402 Scanning electron microscopy (SEM) 12 μm |
|
Micrograph
643
:
Aligned carbon nanotubes, coated with a conducting polymer System: Carbon nanotube, Composition: Coating of polypyrrole Scanning electron microscopy (SEM) 1 μm |
|
Micrograph
644
:
Carbon nanotubes, coated with a conducting polymer System: Carbon nanotube, Composition: Coating of polypyrrole Scanning electron microscopy (SEM) 100 nm |
|
Micrograph
799
:
Austenitic stainless steel solution treated, water quenched and tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Scanning electron microscopy (SEM) 2 μm |
Showing 61 - 70 of 87 micrographs | Page 1 .. 3 4 5 6 7 8 9 | Previous | Next |