31 micrographs for technique Transmission electron microscopy (TEM), ordered by micrograph number.


Showing 21 - 30 of 31 micrographs Page 1 2 3 4 | Previous | Next

Link to full record for micrograph 814 Micrograph 814 : Austenitic stainless steel solution treated, quenched and tempered
System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%)
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 816 Micrograph 816 : Austenitic stainless steel solution treated, quenched and tempered, showing M23C6 precipitate
System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Mo 1 (wt%)
Transmission electron microscopy (TEM)
400 nm
Link to full record for micrograph 822 Micrograph 822 : Austenitic stainless steel tempered
System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%)
Transmission electron microscopy (TEM)
400 nm
Link to full record for micrograph 823 Micrograph 823 : Martensitic steel tempered, with dislocation helices in ferrite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 824 Micrograph 824 : Martensitic steel tempered, with precipitation of Mo2C in ferrite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 827 Micrograph 827 : Martensitic steel quenched then tempered
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 828 Micrograph 828 : Martensitic steel tempered, with precipitation of Mo2C on dislocations in ferrite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
500 nm
Link to full record for micrograph 829 Micrograph 829 : Martensitic steel quenched then tempered, with precipitation of Mo2C on dislocations in ferrite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
500 nm
Link to full record for micrograph 830 Micrograph 830 : Martensitic steel tempered, with precipitation of Mo2C on dislocations
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
2 μm
Link to full record for micrograph 832 Micrograph 832 : Austenitic stainless steel tempered
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
200 nm