Link to full record for micrograph 835 Micrograph 835 : Martensitic steel tempered, with precipitation of Mo2C
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
1 μm