Re-use of this resource is governed by a Creative Commons
Attribution-
NonCommercial-ShareAlike 4.0 International
https://creativecommons.org/licenses/by-nc-sa/4.0/
This is the Tafel plot for a single electrode.
Roll over the upper parts of the graph to see an explanation.
This reduction reaction has the form Mz+ +
ze− → M