Re-use of this resource is governed by a Creative Commons
Attribution-
NonCommercial-ShareAlike 4.0 International
https://creativecommons.org/licenses/by-nc-sa/4.0/
Cyclically deformed austenitic stainless steel. AISI 304LN:
C 0.03, Mn 1.78, Si 0.65, S 0.02, P 0.034, Ni 8.17,
Cr 18.73, Mo 0.26, Cu 0.29, N 0.08 and the balance Fe (wt%)
Image reproduced with permission of Arpan Das, Scientist, Materials
Science & Technology Division,
National Metallurgical Laboratory, Jamshedpur, India
Select a grain within the image above by clicking on it
Selected
grain colour
The colour corresponds to the three Euler angles between
the crystallographic axes and the external frame of reference.
X1, X2 and X3 are axes defined by the
external frame of reference.
The Euler angles are calculated using the Bunge convention (see Representing
Texture 2 section).