b: 3.61 /Å
d: 3.61 /Å
The value of the ratio b/d is 1.00
G: 46.2 GPa
v: 0.3
w/b: 0.789
Select a material to see the plot:
The Peierls energy is the magnitude of the energy at the maximum (i.e. where α = ∓ 0.25). So now the Peierls energy is 0.88 x 10 -13 J m-1