TLP Library
Teaching and learning packages (TLPs) are self-contained, interactive resources, each focusing on one area of Materials Science.
Despite undergoing a process to update our older TLPs over the last year or more, many of our TLPs still contain Flash animations. These are highlighted in the list below (). Unfortunately with Flash being End-Of-Life they no longer work. Please be reassured that we are continuing the process over the coming month. Any TLPs listed below that do not have a Flash animation tag either have no animations within them or the animations have been created using HTML5 (
). We have found that often the HTML5 animations render better in Microsoft Edge, so if your favourite browser does not work very well with them, please try an alternative.
Search for a TLP
- alloys(8)
- atomic-scale structure(19)
- ceramics(4)
- chemistry(5)
- composites(5)
- corrosion(2)
- crystallinity(5)
- crystallography(7)
- diffraction(6)
- diffusion(6)
- elastic deformation(8)
- electronic properties(8)
- energy(3)
- experiment(10)
- failure(5)
- Finite Element Method(3)
- fluid dynamics(1)
- functional materials(8)
- fundamentals(6)
- kinetics(5)
- magnetism(2)
- manufacturing(6)
- mechanical properties(20)
- metals(16)
- microscopy(8)
- microstructure(6)
- optical properties(5)
- phase transformations(7)
- plastic deformation(9)
- polymers(9)
- Raman spectroscopy(1)
- steel(3)
- tensors(4)
- thermal properties(4)
- thermodynamics(7)
- thin films(4)
Toggle TLP descriptions
Currently showing 6 TLPs
Having the following tags:
Avoidance of Crystallization in Biological Systems
This teaching and learning package discusses the two main environmental threats leading to crystallization in plants and animals, and the ways in which organisms have adapted to avoid this crystallization. As part of this discussion, there is coverage of some of the theory of nucleation and crystallization.
Elasticity in Biological Materials
This teaching and learning package (TLP) discusses the elasticity of biological materials. Whilst some show Hookean elasticity, the vast majority do not. Non-linear elasticity is considered, in particular J-shaped and S-shaped curves. Viscoelasticity is also discussed, using hair and spiders' silk as examples.
Granular Materials
This teaching and learning package (TLP) is an introduction to the static behaviour and flow behaviour of granular materials.
Optimisation of Materials Properties in Living Systems
This teaching and learning package discusses the uses of merit indices in conjunction with materials-selection maps focusing on biomaterials. The derivation of merit indices is discussed and biological examples are shown.
The Structure and Mechanical Behaviour of Wood
This teaching and learning package discusses the structure of wood, focusing on the structure of the tree trunk and the differences between hardwoods and softwoods. The stiffness and strength of different types of wood are discussed, and the different behaviour of wood when wet is investigated.
Structure of Bone and Implant Materials
This teaching and learning package (TLP) describes the structure of bone from the macro-scale to the micro-scale and considers its description as a biological composite. The structure of hip replacements is described and common implant materials are discussed in relation to the mechanical properties of bone.