Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

DoITPoMS TLP Library

TLP Library

Teaching and learning packages (TLPs) are self-contained, interactive resources, each focusing on one area of Materials Science.

TLPs containing HTML5 animations/simulations are labelled with the tag . We have found that often the HTML5 animations render better in Microsoft Edge, so if your favourite browser does not work very well with them, please try an alternative.

Batteries

This TLP investigates the basic principles, design and applications of batteries. It covers both primary and rechargeable batteries, how they work and how they may be used.

Crystallographic Texture

This teaching and learning package (TLP) introduces the concept of texture in crystalline materials such as common metals and metallic alloys.

Diffraction and Imaging

A brief summary of diffraction and imaging using an optical system.

Ellingham Diagrams

The Ellingham diagram is a tool most often used in extraction metallurgy to find the conditions necessary for the reduction of the ores of important metals. This Teaching and Learning Package incorporates an interactive Ellingham diagram. This diagram can be used to quickly and simply find a range of thermodynamic data relating to many metallurgical reactions.

Fuel Cells

This teaching and learning package provides a short summary of four of the most promising fuel cell technologies. It gives a general overview of the field with focus on materials used (electrolytes and electrodes) and the mechanism of function (electrochemistry and thermodynamics).

The Glass Transition in Polymers

This teaching and learning package is based on a lecture demonstrations used within the Department of Materials Science and Metallurgy at the University of Cambridge. The package is aimed at first year undergraduate Materials Science students and focuses on the glass transition in polymers.

Indexing Electron Diffraction Patterns

An introduction to the indexing of diffraction patterns.

The Nernst Equation and Pourbaix Diagrams

This teaching and learning package (TLP) investigates the Nernst equation and Pourbaix diagrams, which are both important parts of electrochemistry and corrosion science.

Phase Diagrams and Solidification

Phase diagrams are a useful tool in metallurgy and other branches of materials science. They show the mixture of phases present in thermodynamic equilibrium. This teaching and learning package looks at the theory behind phase diagrams, and ways of constructing them, before running through an experimental procedure, and presenting the results which can be obtained.

Reciprocal Space

This TLP shows the construction of reciprocal lattices from real ones, use of the Ewald sphere for diffraction experiments and some other applications of reciprocal space.

Solid Solutions

This teaching and learning package is based on a practical used within the Department of Materials Science and Metallurgy at the University of Cambridge. The package is aimed at first year undergraduate Materials Science students and focuses on the different types of solid solution and the thermodynamic principles involved in understanding them.

The Stereographic Projection

This TLP covers the use of the Stereographic projection and Wulff nets.

X-ray Diffraction Techniques

This teaching & learning package provides an introduction to X-ray diffraction. It describes the main crystallographic information that can be obtained and experimental methods most commonly used.