2.The Yield Point is the stress level at which plastic deformation first occurs.
3.Plastic Flow. Slip occurs on glide planes by the passage of dislocations.
4.Elastic strain recovery. Non-permanent elastic deformation is recovered upon release of a mechanical stress.