AimsBefore you startIntroductionLévy-Mises Equations• Plane stress• Plane strainSlip Line Field TheoryWork Formula MethodLimit Analysis• Notched bar in tension• Notched bar in plane bending• Hodographs I• Hodographs IIFinite Element MethodSummaryQuestionsGoing furtherTLP creditsTLP contentsShow all contentViewing and downloading resourcesAbout the TLPsTerms of useFeedbackCredits Print this page
PreviousNext
Aims
- Appreciate different approaches, including their inherent assumptions, that can be used to model plastic flow in metal forming operations.
- Gain an insight into these approaches and how they can provide estimates of the necessary deformation loads for different metal forming operations.
- Recognise the relative importance and limitations of the different approaches, ranging from simple work analyses to hodographs, and to become familiar with their use.