AimsBefore you startIntroductionPowder particles in a fluid streamParticle size measurement by light scatteringParticle impact on substratesCase study - thermal sprayingPassage of particles through filterDiesel particulate filtersPowder consolidation by cold pressing and sinteringSummaryQuestionsGoing furtherTLP creditsTLP contentsShow all contentViewing and downloading resourcesAbout the TLPsTerms of useFeedbackCredits Print this page
PreviousNext
Aims
On completion of this TLP you should:
- Understand the factors that control the dynamics of solid particles in fluids
- Be familiar with the main method for measurement of particle size distribution
- Be able to make simple calculations relating to the flow of fluids through permeable media, such as filters
- Understand how powders are commonly handled and processed to make solid artefacts or surface coatings