1. Select metal
2.
3.
4. Enter displacement
5.
to graph
6.
\[ E = \frac{1}{3}\frac{g\times L^{3}}{gradient\times
I} \] \[ E = \frac{1}{3}\frac{9,8\times 0.15^{3}}{gradient\times 8.3\times
10^{-13}} \]
7. Drag line for the best gradient.
\[ E = \frac{1}{3}\frac{9.8\times 0.15^{3}}{\qquad\quad\times
8.3\times 10^{-13}} \]