11 micrographs for composition Fe, C 0.2, Mo 4 (wt%), ordered by micrograph number.

Showing 1 - 10 of 11 micrographs Page 1 2 | Previous | Next

Link to full record for micrograph 807 Micrograph 807 : Martensitic steel solution treated and rapidly cooled with dislocation in retained autenite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
500 nm
Link to full record for micrograph 808 Micrograph 808 : Martensitic steel tempered with precipitation of Mo2C
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
200 nm
Link to full record for micrograph 815 Micrograph 815 : Martensitic steel, lightly rolled, with dislocations in austenite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Scanning electron microscopy (SEM)
400 nm
Link to full record for micrograph 823 Micrograph 823 : Martensitic steel tempered, with dislocation helices in ferrite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 824 Micrograph 824 : Martensitic steel tempered, with precipitation of Mo2C in ferrite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 827 Micrograph 827 : Martensitic steel quenched then tempered
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 828 Micrograph 828 : Martensitic steel tempered, with precipitation of Mo2C on dislocations in ferrite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
500 nm
Link to full record for micrograph 829 Micrograph 829 : Martensitic steel quenched then tempered, with precipitation of Mo2C on dislocations in ferrite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
500 nm
Link to full record for micrograph 830 Micrograph 830 : Martensitic steel tempered, with precipitation of Mo2C on dislocations
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
2 μm
Link to full record for micrograph 832 Micrograph 832 : Austenitic stainless steel tempered
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
200 nm

Showing 1 - 10 of 11 micrographs Page 1 2 | Previous | Next