Link to full record for micrograph 777 Micrograph 777 : Grey cast iron (flake graphite)
System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 778 Micrograph 778 : Grey cast iron (flake graphite)
System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 779 Micrograph 779 : Spheroidal graphite cast iron
System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%)
Reflected light microscopy
50 μm
Link to full record for micrograph 780 Micrograph 780 : Heat treated spheroidal graphite cast iron
System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 781 Micrograph 781 : Heat treated spheroidal graphite cast iron
System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%)
Reflected light microscopy
50 μm
Link to full record for micrograph 782 Micrograph 782 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 783 Micrograph 783 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 784 Micrograph 784 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 785 Micrograph 785 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
20 μm
Link to full record for micrograph 786 Micrograph 786 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)