DoITPoMS

Keyword

71 micrographs for keyword polymer, ordered by micrograph number.


Showing 51 - 60 of 71 micrographs Page 1 2 3 4 5 6 7 8 | Previous | Next

Link to full record for micrograph 612 Micrograph 612 : Nematic liquid crystalline polymer
System: Liquid crystalline polymer, Composition: K24 (4-cyano-4'-8-alkylbiphenyl)
Cross-polarised light microscopy
100 μm
Link to full record for micrograph 618 Micrograph 618 : Fracture surface of a carbon fibre composite
System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
600 μm
Link to full record for micrograph 620 Micrograph 620 : Kevlar fibre composite fracture surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
600 μm
Link to full record for micrograph 621 Micrograph 621 : Kevlar fibre composite shear surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 622 Micrograph 622 : Kevlar fibre composite shear surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 625 Micrograph 625 : Series of laser welds in amorphous PET
System: Polyethylene terephthalate (PET), Composition: Amorphous polyethylene terephthalate (APET)
Cross-polarised light microscopy
12 mm
Link to full record for micrograph 626 Micrograph 626 : Glass fibre reinforced thermoplastic matrix composite
System: Glass fibre composite, Composition: Polypropylene matrix with glass fibre
Scanning electron microscopy (SEM)
60 μm
Link to full record for micrograph 627 Micrograph 627 : Glass fibre reinforced thermoplastic matrix composite
System: Glass fibre composite, Composition: Polypropylene matrix with glass fibre
Scanning electron microscopy (SEM)
200 μm
Link to full record for micrograph 637 Micrograph 637 : Disclinations in a smectic LCP, revealed by decoration
System: Liquid crystalline polymer, Composition: Semi-flexible LCP, Cl-7
Cross-polarised light microscopy
10 μm
Link to full record for micrograph 638 Micrograph 638 : Disclinations in a smectic LCP, revealed by decoration
System: Liquid crystalline polymer, Composition: Semi-flexible LCP, Cl-8
Cross-polarised light microscopy
10 μm

Showing 51 - 60 of 71 micrographs Page 1 2 3 4 5 6 7 8 | Previous | Next

List all keywords