Keyword
1 micrograph for keyword Saffil, ordered by micrograph number.
Micrograph
606
:
Extruded Saffil-containing metal matrix composite System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |