Link to full record for micrograph 31 Micrograph 31 : Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 32 Micrograph 32 : Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 33 Micrograph 33 : Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 34 Micrograph 34 : Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 35 Micrograph 35 : Cu 70, Zn 30 (wt%), faster recrystallisation - finer grain size
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 37 Micrograph 37 : Cu 70, Zn 30 (wt%), slow cooling - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 38 Micrograph 38 : Cu 98, Be 2 (wt%), slow cooling - annealing twins
System: Cu-Be, Composition: Cu 98, Be 2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 156 Micrograph 156 : Roll-bonded aluminium alloy diffusion couple annealed for 30 minutes at 600ºC.
System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%)
Cross-polarised light microscopy
400 μm
Link to full record for micrograph 157 Micrograph 157 : Roll-bonded aluminium alloy diffusion couple annealed for 60 minutes at 600ºC.
System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%)
Cross-polarised light microscopy
750 μm
Link to full record for micrograph 211 Micrograph 211 : Normalised carbon steel
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
400 μm