Link to full record for micrograph 397 Micrograph 397 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy, polarised
400 μm
Link to full record for micrograph 398 Micrograph 398 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
200 μm
Link to full record for micrograph 399 Micrograph 399 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
100 μm
Link to full record for micrograph 400 Micrograph 400 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
400 μm
Link to full record for micrograph 401 Micrograph 401 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
100 μm
Link to full record for micrograph 402 Micrograph 402 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
100 μm
Link to full record for micrograph 403 Micrograph 403 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
400 μm
Link to full record for micrograph 404 Micrograph 404 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
200 μm
Link to full record for micrograph 405 Micrograph 405 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
100 μm
Link to full record for micrograph 406 Micrograph 406 : Cast iron, containing phosphorus
System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%)
Reflected light microscopy
800 μm