Keyword
31 micrographs for keyword bismuth, ordered by micrograph number.
Showing 1 - 10 of 31 micrographs | Page 1 2 3 4 | Previous | Next |
Micrograph
6
:
Bi 60, Cd 40 (wt%), eutectic alloy System: Bi-Cd, Composition: Bi 60, Cd 40 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
7
:
Bi 60, Cd 40 (wt%), eutectic alloy System: Bi-Cd, Composition: Bi 60, Cd 40 (wt%) Reflected light microscopy 40 μm |
|
Micrograph
8
:
Bi 80, Cd 20 (wt%), hypereutectic alloy System: Bi-Cd, Composition: Bi 80, Cd 20 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
9
:
Bi 80, Cd 20 (wt%), hypereutectic alloy System: Bi-Cd, Composition: Bi 80, Cd 20 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
744
:
Bi 10, Sn 90 (wt%) System: Bi-Sn, Composition: Bi 10, Sn 90 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 300 μm |
|
Micrograph
745
:
Bi 10, Sn 90 (wt%) System: Bi-Sn, Composition: Bi 10, Sn 90 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 100 μm |
|
Micrograph
746
:
Bi 10, Sn 90 (wt%) System: Bi-Sn, Composition: Bi 10, Sn 90 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 10 μm |
|
Micrograph
747
:
Bi 20, Sn 80 (wt%) System: Bi-Sn, Composition: Bi 20, Sn 80 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 300 μm |
|
Micrograph
748
:
Bi 20, Sn 80 (wt%) System: Bi-Sn, Composition: Bi 20, Sn 80 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 100 μm |
|
Micrograph
749
:
Bi 20, Sn 80 (wt%) System: Bi-Sn, Composition: Bi 20, Sn 80 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 10 μm |
Showing 1 - 10 of 31 micrographs | Page 1 2 3 4 | Previous | Next |