Micrograph 82 and full record
- Micrograph no
- 82
- Brief description
- Aluminium, fracture surface
- Keywords
- alloy , aluminium , fracture , metal
- Categories
- Fracture, Metal or alloy
- System
- Al
- Composition
- Not specified
- Standard codes
- Reaction
- Processing
- Applications
- Sample preparation
- Technique
- Scanning electron microscopy (SEM)
- Length bar
- 15 μm
- Further information
- Contributor
- Prof T W Clyne
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 25/10/01
- Licence for re-use
- Attribution-NonCommercial-ShareAlike 4.0 International
- Related micrographs
View image alone .. in a new window
Help is available on downloading images