Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

System

333 micrographs for system Fe-C-X, ordered by micrograph number.


Showing 241 - 250 of 333 micrographs Page 1 .. 22 23 24 25 26 27 28 .. 34 | Previous | Next

Link to full record for micrograph 413 Micrograph 413 : Cast iron, containing phosphorus
System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 414 Micrograph 414 : Cast iron, containing phosphorus
System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 415 Micrograph 415 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
800 μm
Link to full record for micrograph 416 Micrograph 416 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
200 μm
Link to full record for micrograph 417 Micrograph 417 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy, polarised with wave-plate
800 μm
Link to full record for micrograph 418 Micrograph 418 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
400 μm
Link to full record for micrograph 419 Micrograph 419 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
100 μm
Link to full record for micrograph 735 Micrograph 735 : Dual-phase steel water quenched from 750°C
System: Fe-C-X, Composition: Fe, C 0.15, Mn 1.5, Si 1.5 (wt%)
Reflected light microscopy
6 μm
Link to full record for micrograph 736 Micrograph 736 : Dual-phase steel water quenched from 775°C
System: Fe-C-X, Composition: Fe, C 0.15, Mn 1.5, Si 1.5 (wt%)
Reflected light microscopy
5 μm
Link to full record for micrograph 737 Micrograph 737 : Dual-phase steel water quenched from 800°C
System: Fe-C-X, Composition: Fe, C 0.15, Mn 1.5, Si 1.5 (wt%)
Reflected light microscopy
6 μm

Showing 241 - 250 of 333 micrographs Page 1 .. 22 23 24 25 26 27 28 .. 34 | Previous | Next