333 micrographs for system Fe-C-X, ordered by micrograph number.
Showing 251 - 260 of 333 micrographs | Page 1 .. 23 24 25 26 27 28 29 .. 34 | Previous | Next |
Micrograph
738
:
A medium carbon low alloyed structural steel System: Fe-C-X, Composition: Fe, C medium (wt%), with small alloy addition Reflected light microscopy 20 μm |
|
Micrograph
739
:
TRIP steel annealed at 775°C for 5 mins and then hold at 400°C for 150s for austenite stabilization System: Fe-C-X, Composition: Fe, C 0.15, Mn 1.5, Si 1.5 (wt%) Reflected light microscopy 6 μm |
|
Micrograph
740
:
TRIP steel annealed at 775°C for 5 mins and then hold at 400°C for 40s for austenite stabilization System: Fe-C-X, Composition: Fe, C 0.15, Mn 1.5, Si 1.5 (wt%) Reflected light microscopy 20 μm |
|
Micrograph
741
:
A medium carbon low alloyed structural steel System: Fe-C-X, Composition: Fe, C medium (wt%), with small alloy addition Reflected light microscopy 30 μm |
|
Micrograph
742
:
A medium carbon low alloyed structural steel System: Fe-C-X, Composition: Fe, C medium (wt%), with small alloy addition Reflected light microscopy 20 μm |
|
Micrograph
743
:
A medium carbon low alloyed structural steel System: Fe-C-X, Composition: Fe, C medium (wt%), with small alloy addition Reflected light microscopy 6 μm |
|
Micrograph
771
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Reflected light microscopy 100 μm |
|
Micrograph
772
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Transmission electron microscopy (TEM) 1 μm |
|
Micrograph
773
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Transmission electron microscopy (TEM) 1 μm |
|
Micrograph
774
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Transmission electron microscopy (TEM) 1 μm |