Technique
87 micrographs for technique Scanning electron microscopy (SEM), ordered by micrograph number.
| Showing 41 - 50 of 87 micrographs | Page 1 2 3 4 5 6 7 8 9 | Previous | Next |
![]() |
Micrograph
584
:
External surface of blow-moulded HDPE System: High density polyethylene (HDPE), Composition: Not specified Scanning electron microscopy (SEM) 400 μm |
![]() |
Micrograph
585
:
Internal surface of blow-moulded HDPE System: High density polyethylene (HDPE), Composition: Not specified Scanning electron microscopy (SEM) 6 μm |
![]() |
Micrograph
586
:
Fracture surface in polystyrene System: Polystyrene (PS), Composition: Not specified Scanning electron microscopy (SEM) 160 μm |
![]() |
Micrograph
587
:
Parabolic beach marks on a polystyrene fracture surface System: Polystyrene (PS), Composition: Not specified Scanning electron microscopy (SEM) 80 μm |
![]() |
Micrograph
588
:
Beach marks on a polystyrene fracture surface System: Polystyrene (PS), Composition: Not specified Scanning electron microscopy (SEM) 50 μm |
![]() |
Micrograph
589
:
Remnants of crazes on a polystyrene fracture surface System: Polystyrene (PS), Composition: Not specified Scanning electron microscopy (SEM) 8 μm |
![]() |
Micrograph
590
:
Remnants of crazes on a polycarbonate fracture surface System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 10 μm |
![]() |
Micrograph
591
:
Crazing near a fracture surface in polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 80 μm |
![]() |
Micrograph
592
:
The tip of a craze in polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
593
:
Ductile tearing near a fracture surface in polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 100 μm |
| Showing 41 - 50 of 87 micrographs | Page 1 2 3 4 5 6 7 8 9 | Previous | Next |