1 micrograph for technique Reflected light microscopy, polarised with wave-plate, ordered by micrograph number.


Link to full record for micrograph 417 Micrograph 417 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy, polarised with wave-plate
800 μm