On completion of this tutorial you should:
- Be aware of major deformation processes and the ways in which they are used to form metallic objects:
- Rolling
- Extrusion
- Forging
- Drawing
- Appreciate the advantages and disadvantages of each.
- Understand the reasons for selecting a process for a particular shape of end product.

© 2004-2012 University of Cambridge.