172 micrographs for keyword steel, ordered by micrograph number.


Showing 61 - 70 of 172 micrographs Page 1 .. 4 5 6 7 8 9 10 .. 18 | Previous | Next

Link to full record for micrograph 239 Micrograph 239 : Fe, C 0.4, Mn 0.8 (wt%) steel, normalised
System: Fe-C-X, Composition: Fe, C 0.4, Mn 0.8 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 240 Micrograph 240 : Fe, C 0.4, Mn 0.8 (wt%) steel, normalised
System: Fe-C-X, Composition: Fe, C 0.4, Mn 0.8 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 241 Micrograph 241 : Fe, C 0.3 (wt%) steel, spheroidised carbide
System: Fe-C-X, Composition: Fe, C 0.3 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 242 Micrograph 242 : Fe, C 0.3 (wt%) steel, spheroidised carbide
System: Fe-C-X, Composition: Fe, C 0.3 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 243 Micrograph 243 : Fe, C 1.3 (wt%) steel, annealed at 1100°C
System: Fe-C-X, Composition: Fe, C 1.3 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 244 Micrograph 244 : Fe, C 1.3 (wt%) steel, annealed at 1100°C
System: Fe-C-X, Composition: Fe, C 1.3 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 245 Micrograph 245 : Fe, C 1.3 (wt%) steel, normalised at 1050°C
System: Fe-C-X, Composition: Fe, C 1.3 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 246 Micrograph 246 : Fe, C 1.3 (wt%) steel, normalised at 1050°C
System: Fe-C-X, Composition: Fe, C 1.3 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 247 Micrograph 247 : Fe, C 1.3 (wt%) steel, normalised at 1050°C
System: Fe-C-X, Composition: Fe, C 1.3 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 248 Micrograph 248 : Fe, C 1.3 (wt%) steel, annealed at 1000°C
System: Fe-C-X, Composition: Fe, C 1.3 (wt%)
Reflected light microscopy
400 μm