Categories > Metal or alloy > Fe, C 3.4, Si 0.35, Mn 0.22 (wt%), + ...
3 micrographs available, ordered by micrograph number.
![]() |
Micrograph
365
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%), + ... Reflected light microscopy 200 μm |
![]() |
Micrograph
366
:
Whiteheart cast iron System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%), + ... Reflected light microscopy 400 μm |
![]() |
Micrograph
367
:
Whiteheart cast iron System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%), + ... Reflected light microscopy 200 μm |