Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Metal or alloy > Cu 80, Zn 20 (wt%)
6 micrographs available, ordered by micrograph number.
![]() |
Micrograph
431
:
Cu 80, Zn 20 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
432
:
Cu 80, Zn 20 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
477
:
Cu 80, Zn 20 (wt%) brass, exhibiting dendritic solidification System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
478
:
Cu 80, Zn 20 (wt%) brass, exhibiting dendritic solidification System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
479
:
Cu 80, Zn 20 (wt%) brass, exhibiting dendritic solidification System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
480
:
Cu 80, Zn 20 (wt%) brass, exhibiting dendritic solidification System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 100 μm |
Help is available on browsing.