Categories > Metal or alloy > Cu 46, Zn 42, Ni 10, Pb 2 (wt%) > Keyword: brass

2 micrographs available, ordered by micrograph number.


Link to full record for micrograph 439 Micrograph 439 : a b nickel brass containing 2% lead.
System: Cu-Zn, Composition: Cu 46, Zn 42, Ni 10, Pb 2 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 440 Micrograph 440 : a b nickel brass containing 2% lead.
System: Cu-Zn, Composition: Cu 46, Zn 42, Ni 10, Pb 2 (wt%)
Reflected light microscopy
400 μm