Categories > Metal or alloy > Cu 60, Zn 40 (wt%)
2 micrographs available, ordered by micrograph number.
![]() |
Micrograph
441
:
Cu 60, Zn 40 (wt%) brass, Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
442
:
Cu 60, Zn 40 (wt%) brass, Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 100 μm |