Categories > Metal or alloy > Cu 85, Sn 10, Pb 5 (wt% approx) > Reflected light microscopy > Keyword: bronze

3 micrographs available, ordered by micrograph number.


Link to full record for micrograph 509 Micrograph 509 : D4 Leaded bronze, cored dendrites.
System: Cu-Sn, Composition: Cu 85, Sn 10, Pb 5 (wt% approx)
Reflected light microscopy
400 μm
Link to full record for micrograph 510 Micrograph 510 : D4 Leaded bronze, cored dendrites.
System: Cu-Sn, Composition: Cu 85, Sn 10, Pb 5 (wt% approx)
Reflected light microscopy
200 μm
Link to full record for micrograph 511 Micrograph 511 : D4 Leaded bronze, cored dendrites.
System: Cu-Sn, Composition: Cu 85, Sn 10, Pb 5 (wt% approx)
Reflected light microscopy
100 μm