Categories > Metal or alloy > Cu 85, Sn 5, Zn 5, Pb 5 (wt% approx)
4 micrographs available, ordered by micrograph number.
![]() |
Micrograph
512
:
Leaded gun metal bronze. System: Cu-Sn, Composition: Cu 85, Sn 5, Zn 5, Pb 5 (wt% approx) Reflected light microscopy 800 μm |
![]() |
Micrograph
513
:
Leaded gun metal bronze. System: Cu-Sn, Composition: Cu 85, Sn 5, Zn 5, Pb 5 (wt% approx) Reflected light microscopy 200 μm |
![]() |
Micrograph
514
:
Leaded gun metal bronze. System: Cu-Sn, Composition: Cu 85, Sn 5, Zn 5, Pb 5 (wt% approx) Reflected light microscopy 100 μm |
![]() |
Micrograph
515
:
Leaded gun metal bronze. System: Cu-Sn, Composition: Cu 85, Sn 5, Zn 5, Pb 5 (wt% approx) Reflected light microscopy 400 μm |