Browse the Library
Categories > Metal or alloy > Fe, C 0.2 (wt%)
8 micrographs available, ordered by micrograph number.
![]() |
Micrograph
43
:
Fe, C 0.2 (wt%), explosively deformed - mechanical twins System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
44
:
Fe, C 0.2 (wt%), explosively deformed - mechanical twins System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
207
:
Normalised low carbon manganese steel, taken transverse to directionality System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
208
:
Normalised low carbon manganese steel, taken transverse to directionality System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
209
:
As cast carbon steel System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
210
:
As cast carbon steel System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
211
:
Normalised carbon steel System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
212
:
Normalised carbon steel System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 200 μm |