Browse the Library
Categories > Metal or alloy > Al, Si 12, Na 0.02 (wt%)
2 micrographs available, ordered by micrograph number.
![]() |
Micrograph
60
:
Al, Si 12, Na 0.02 (wt%), eutectic alloy - refined microstructure System: Al-Si-Na, Composition: Al, Si 12, Na 0.02 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
61
:
Al, Si 12, Na 0.02 (wt%), eutectic alloy - refined microstructure System: Al-Si-Na, Composition: Al, Si 12, Na 0.02 (wt%) Reflected light microscopy 80 μm |