Categories > Metal or alloy > Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) > Scanning electron microscopy (SEM)
1 micrograph available, ordered by micrograph number.
Micrograph
799
:
Austenitic stainless steel solution treated, water quenched and tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Scanning electron microscopy (SEM) 2 μm |