Categories > Metal or alloy > Fe, Mn 1, S 0.02 (wt%)
1 micrograph available, ordered by micrograph number.
![]() |
Micrograph
810
:
Ferritic steel heat treated and water quenched System: Fe-C-X, Composition: Fe, Mn 1, S 0.02 (wt%) Scanning electron microscopy (SEM) 1.5 μm |