Browse the Library
Categories > Metal or alloy > Fe, C 0.13, Ni 4, Cr 2, Mn 0.49, S 0.015 (wt%)
3 micrographs available, ordered by micrograph number.
![]() |
Micrograph
811
:
Austenitic stainless steel rapidly cooled, fracture surface of laboratory ingot System: Fe-C-X, Composition: Fe, C 0.13, Ni 4, Cr 2, Mn 0.49, S 0.015 (wt%) Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
812
:
Austenitic stainless steel rapidly cooled, fracture surface of laboratory ingot System: Fe-C-X, Composition: Fe, C 0.13, Ni 4, Cr 2, Mn 0.49, S 0.015 (wt%) Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
834
:
Steel slowly cooled, fracture surface of commercial ingot System: Fe-C-X, Composition: Fe, C 0.13, Ni 4, Cr 2, Mn 0.49, S 0.015 (wt%) Scanning electron microscopy (SEM) 4 μm |