Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Metal or alloy > Stainless steel with Cr 18, Ni 10, Mo 1 (wt%)
2 micrographs available, ordered by micrograph number.
![]() |
Micrograph
813
:
Austenitic stainless steel solution treated, quenched and tempered, with M23C6 precipitate System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Mo 1 (wt%) Transmission electron microscopy (TEM) 400 nm |
![]() |
Micrograph
816
:
Austenitic stainless steel solution treated, quenched and tempered, showing M23C6 precipitate System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Mo 1 (wt%) Transmission electron microscopy (TEM) 400 nm |