Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Metal or alloy > Fe, C 1.15, Mn 13 (wt%)
1 micrograph available, ordered by micrograph number.
![]() |
Micrograph
821
:
Austenitic stainless steel impact deformed at room temperature System: Fe-C-X, Composition: Fe, C 1.15, Mn 13 (wt%) Scanning electron microscopy (SEM) 2.5 μm |