Browse the Library
Categories > Metal or alloy > Not specified (Fe production) > Transmitted light microscopy
7 micrographs available, ordered by micrograph number.
Micrograph
909
:
Joldelund, Germany. Iron slag System: Fe production, Composition: Not specified Transmitted light microscopy 1 mm |
|
Micrograph
925
:
Wissenbach, Westerwald, Germany. Iron slag System: Fe production, Composition: Not specified Transmitted light microscopy 200 μm |
|
Micrograph
926
:
Wissenbach, Westerwald, Germany. Iron slag System: Fe production, Composition: Not specified Transmitted light microscopy 500 μm |
|
Micrograph
927
:
Wissenbach, Westerwald, Germany. Iron slag System: Fe production, Composition: Not specified Transmitted light microscopy 500 μm |
|
Micrograph
950
:
Haus Rhade, Sauerland, Germany. Subrecent Fe-production System: Fe production, Composition: Not specified Transmitted light microscopy 1 mm |
|
Micrograph
951
:
Haus Rhade, Sauerland, Germany. Subrecent Fe-production System: Fe production, Composition: Not specified Transmitted light microscopy 500 μm |
|
Micrograph
960
:
Fichtel mountain, Germany. Subrecent iron slag System: Fe production, Composition: Not specified Transmitted light microscopy 200 μm |
Help is available on browsing.