Browse the Library
Categories > Metal or alloy > Not specified (Fe-C-X)
3 micrographs available, ordered by micrograph number.
![]() |
Micrograph
143
:
Notched low carbon ferritic steel, failed through cleavage. System: Fe-C-X, Composition: Not specified Scanning electron microscopy (SEM) 20 μm |
![]() |
Micrograph
146
:
HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture. System: Fe-C-X, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
![]() |
Micrograph
147
:
HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture. System: Fe-C-X, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |