Browse the Library
Categories > Metal or alloy > Fe, C 0.15 (wt%)
7 micrographs available, ordered by micrograph number.
![]() |
Micrograph
286
:
Fe, C 0.15 (wt%) steel, carburised System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
287
:
Fe, C 0.15 (wt%) steel, carburised System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
288
:
Fe, C 0.15 (wt%) steel, carburised System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
289
:
Fe, C 0.15 (wt%) steel, carburised System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
350
:
Fe, C 0.15 (wt%) steel, quenched. System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
351
:
Fe, C 0.15 (wt%) steel, quenched. System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
352
:
Fe, C 0.15 (wt%) steel, quenched. System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 100 μm |