Categories > Metal or alloy > Keyword: coring
16 micrographs available, ordered by micrograph number.
Showing 11 - 16 of 16 micrographs | Page 1 2 | Previous | Next |
Micrograph
525
:
Phosphor bronze exhibiting cored dendrites. System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) + P trace Reflected light microscopy 100 μm |
|
Micrograph
695
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
696
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
697
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
698
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
699
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 20 μm |