Categories > Metal or alloy > Keyword: precipitation

10 micrographs available, ordered by micrograph number.


Link to full record for micrograph 56 Micrograph 56 : Al 96, Cu 4 (wt%), solution treated and overaged - precipitation hardening
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 57 Micrograph 57 : Al 96, Cu 4 (wt%), solution treated and overaged - precipitation hardening
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 713 Micrograph 713 : IN718 nickel-based superalloy held for 1 minute at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
20 μm
Link to full record for micrograph 714 Micrograph 714 : IN718 nickel-based superalloy held for 20 minutes at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
20 μm
Link to full record for micrograph 715 Micrograph 715 : IN718 nickel-based superalloy held for 1 hour at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
25 μm
Link to full record for micrograph 716 Micrograph 716 : IN718 nickel-based superalloy held for 3 hours at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
25 μm
Link to full record for micrograph 717 Micrograph 717 : IN718 nickel-based superalloy held for 6 hours at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
25 μm
Link to full record for micrograph 718 Micrograph 718 : IN718 nickel-based superalloy held for 24 hours at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
25 μm
Link to full record for micrograph 719 Micrograph 719 : IN718 nickel-based superalloy held for 48 hours at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
25 μm
Link to full record for micrograph 720 Micrograph 720 : IN718 nickel-based superalloy held for 72 hours at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
25 μm