Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Metal or alloy > Keyword: equiaxed
8 micrographs available, ordered by micrograph number.
![]() |
Micrograph
615
:
Cross-section of an aluminium casting System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy 10 mm |
![]() |
Micrograph
710
:
Wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute); refined with TiB2 particles. Deformation of grain structure is due to cutting of sample with scissors. System: Al-Mg-Fe-Si, Composition: Not specified Cross-polarised light microscopy 400 μm |
![]() |
Micrograph
711
:
As-cast wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute). No addition of grain refinement particles (e.g. TiB2). System: Al-Mg-Fe-Si, Composition: Not specified Cross-polarised light microscopy 1 mm |
![]() |
Micrograph
712
:
As-cast wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute). Addition of TiB2 particles facilitates the formation of a fine, equiaxed grain structure (grain refinement). System: Al-Mg-Fe-Si, Composition: Not specified Cross-polarised light microscopy 400 μm |
![]() |
Micrograph
795
:
Blackheart cast iron System: Fe-C-X, Composition: Blackheart cast iron Reflected light microscopy 100 μm |
![]() |
Micrograph
796
:
Blackheart cast iron System: Fe-C-X, Composition: Blackheart cast iron Reflected light microscopy 100 μm |
![]() |
Micrograph
797
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
798
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 20 μm |