Browse the Library
Categories > Metal or alloy > Keyword: carbide
4 micrographs available, ordered by micrograph number.
![]() |
Micrograph
223
:
Annealed low carbon steel with carbides System: Fe-C-X, Composition: Fe, C low (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
224
:
Annealed low carbon steel with carbides System: Fe-C-X, Composition: Fe, C low (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
797
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
798
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 20 μm |