Browse the Library
Categories > Metal or alloy > Keyword: hypoeutectoid
23 micrographs available, ordered by micrograph number.
Showing 21 - 23 of 23 micrographs | Page 1 2 3 | Previous | Next |
Micrograph
241
:
Fe, C 0.3 (wt%) steel, spheroidised carbide System: Fe-C-X, Composition: Fe, C 0.3 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
242
:
Fe, C 0.3 (wt%) steel, spheroidised carbide System: Fe-C-X, Composition: Fe, C 0.3 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
268
:
Fe, C 0.5 (wt%) steel, near a decarburised surface System: Fe-C-X, Composition: Fe, C 0.5 (wt%) Reflected light microscopy 400 μm |
Showing 21 - 23 of 23 micrographs | Page 1 2 3 | Previous | Next |
Help is available on browsing.