Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Metal or alloy > Keyword: hot tearing
1 micrograph available, ordered by micrograph number.
![]() |
Micrograph
605
:
Fracture surface formed by hot tearing (solidification cracking) System: Al, Composition: Commercial purity (99.5%) Scanning electron microscopy (SEM) 40 μm |