Categories > Metal or alloy > Keyword: pearlite

57 micrographs available, ordered by micrograph number.


Showing 31 - 40 of 57 micrographs Page 1 2 3 4 5 6 | Previous | Next

Link to full record for micrograph 234 Micrograph 234 : Hypoeutectoid steel, normalised at 1100°C
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 235 Micrograph 235 : Hypoeutectoid steel, normalised at 950°C
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 236 Micrograph 236 : Hypoeutectoid steel, normalised at 950°C
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 237 Micrograph 237 : Hypoeutectoid steel, normalised at 950°C
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 238 Micrograph 238 : Hypoeutectoid steel, normalised at 950°C
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 239 Micrograph 239 : Fe, C 0.4, Mn 0.8 (wt%) steel, normalised
System: Fe-C-X, Composition: Fe, C 0.4, Mn 0.8 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 240 Micrograph 240 : Fe, C 0.4, Mn 0.8 (wt%) steel, normalised
System: Fe-C-X, Composition: Fe, C 0.4, Mn 0.8 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 241 Micrograph 241 : Fe, C 0.3 (wt%) steel, spheroidised carbide
System: Fe-C-X, Composition: Fe, C 0.3 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 242 Micrograph 242 : Fe, C 0.3 (wt%) steel, spheroidised carbide
System: Fe-C-X, Composition: Fe, C 0.3 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 777 Micrograph 777 : Grey cast iron (flake graphite)
System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5 (wt%)
Reflected light microscopy
100 μm