Browse the Library
Categories > Metal or alloy > Keyword: annealing
47 micrographs available, ordered by micrograph number.
Showing 31 - 40 of 47 micrographs | Page 1 2 3 4 5 | Previous | Next |
Micrograph
504
:
Cu - 5% Sn bronze, cast annealed. System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%), Reflected light microscopy 800 μm |
|
Micrograph
505
:
Cu - 5% Sn bronze, cast annealed. System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%), Reflected light microscopy 400 μm |
|
Micrograph
506
:
Cu - 5% Sn bronze, cast annealed. System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%), Reflected light microscopy 400 μm |
|
Micrograph
507
:
Annealed 5% Sn bronze. System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%), Reflected light microscopy 200 μm |
|
Micrograph
508
:
Annealed 5% Sn bronze. System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%), Reflected light microscopy 200 μm |
|
Micrograph
526
:
Cast and tempered 20% Sn bronze System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
527
:
Cast and tempered 20% Sn bronze System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
528
:
Cast and tempered 20% Sn bronze System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
529
:
Cast and tempered 20% Sn bronze System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
530
:
Cu - 20% Sn bronze, cast annealed System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 800 μm |
Showing 31 - 40 of 47 micrographs | Page 1 2 3 4 5 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.